Fluid Loss Agent

Fluid Loss Agent

Fluid loss agent is produced by copolymerization of ethylene monomers. It has very good rheology, anti-salt ability and slight dispersing effect, also has good compatibility with API Class G cement and other oil-well cementing additives.

 

Specification

Inspection Items Quality Index
Appearance White powder,

no damping or agglomerating

Density(20±2°C), g/cm3 2.10±0.15
Fineness(0.90mm screen sieve residue), % ≤15
Water content, % ≤8
Slurry Properties Fluid loss(80°C, 6.9MPa, 30min), mL ≤150
Initial consistency, Bc ≤25
Shape of thickening time curve Normal
Transition time from 40Bc to 100Bc, min ≤40
Free fluid, % ≤0.5
Compressive strength(80°C, atm, 24h), MPa ≥14.0
Slurry composition Oil-well cement(HSR): 800g,

FLA-800: 5.5g,

Distilled water: 352g,

Retarder: 0.8g,

Deformer: 0.4g

 

Usage

Application temperature range: 20 – 200°C (BHCT)

Dosage: 0.45-0.55%(BWOC)

 

Packing

Packaged in 25kg moisture-resistant bag.

 

Storage

Stored in dry, normal temperature condition and no direct sun shine. in original packaging away from heat sources. It is recommended to use the product in rotation on a first-in first-out basis.

 

Transportation

During transportation, the products shall be moved gently to prevent damaging the packing bags. Avoid direct contact with Naked flame, when fire happens, any fire fighting equipment may be use to extinguish the fire.

 

Shelf Life

1 year, exceeding valid period, if the products have not lumped and can still be used.

 